Made the purchase yesterday. Bought the smallest bottle and gas and it appears the sales associate realized how old I looked and gave me the "on the 17th green price". I haven't putt out yet so...
Have a couple questions given the first test was so bad, I won't describe it and pictures are out of the question. Actually, nothing welded together, hence the questions.
First, I've thrown enough caution to the wind in my life I decided to take a more conservative approach. Since I like to "see", I did purchase a welding helmet. As I just mentioned about seeing, how do you see thru the thing. That's the first problem. When I tried to make the first tack, I couldn't see a bloody thing. Read the instructions on how to adjust the settings but that didn't make one bit of difference.
Second, I'm following the settings instructions but it doesn't seem "hot" enough. Just little BB's and a long strand of wire but those were able to be removed by hand. Had to describe it after all.
The welder was set at 3.5, just like the chart had shown. Speed was around 2-3. Gas is preset at factory so...
What setting(s) has/have worked for ya'll if using .025 copper coated steel wire?
Also, for testing purposes, I'm dealing with a stainless-steel worktable and lord knows I've been bit severely by our friend the amp a couple times, something I'd like to never experience again. What insulator is best since I do need to clamp the test pieces down? I tried a plastic trigger style clamp held in my vise but it didn't matter because I could see as explained above.
Finally, as far as sizing the actual patch, I purchased the Eastwood tool for butt welds as well as the gap style clamps. The tool is difficult but that may just be the lack of size with the test material. As far as securing the panel exactly where it needs to be, what are some of the methods ya'll have used?